Log homes fail on the south wall first.
UV opens the finish. Water follows the checks. Rot is the last chapter. LogRenewPath turns wall-by-wall condition into a restoration scope you can bid against.

Sun then water, not age.
Inspect the south and west
Those walls write the restoration budget.
Open finish is open water
Wash, then coat. Do not trap moisture.
Logs move
Elastomeric chinking over backer rod, not silicone.
Built like the paperwork it teaches.
A house number hides the failed wall.
We do not invent project photos.
No cut of the job.
This is a new publisher. We do not show customer reviews. The cards above describe how the site is built.
Four ways people arrive.
Owners of 20-year stains
The south wall is already talking.
Buyers of log houses
Condition is not charm. It is a scope.
Cabin caretakers
A maintenance coat is cheaper than a blast.
After a leak
Soft wood under a probe is not a weekend stain.
Direct answers.
Can I just recaulk?
Wide joints on moving logs need chinking designed for that movement.
Is blasting always required?
Only if the finish has failed. Sound stain can be maintained.
Are your costs bids?
No. Planning ranges. Get two written wall-by-wall quotes.